Does H2O improve the catalytic activity of Au1-4/MgO towards CO oxidation?

Martin Amft; Natalia V. Skorodumova · 2011 · arXiv

WASTE classifies this as Negative / Null Result Report · AI classification, approximate

The study found no significant effect — useful as a negative control or null benchmark for your own design.

Abstract (excerpt)

The present density functional theory study addresses the question whether the presence of H2O influences the catalytic activity of small gold clusters, Au1-4/MgO(100), towards the oxidation of carbon monoxide. To this end, we studied the (co-)adsorption of H2O and CO/O2 on these gold clusters. The ground state structures in the presence of all three molecular species, that we found, are Au1O2/MgO and Au2-4CO/MgO with H2O adsorbed on the surface in the proximity of the clusters-molecule complex. In this configuration the catalytic activity of Au1-4/MgO is indifferent to the presence of H2O. We

Excerpt shown for reference under fair use — read the full paper at the publisher.

About to run something similar?

Run an AI Precheck on your own design to catch failure modes like this one before you spend the time. Your first desk check is free.

WASTE indexes this work — it does not host or republish it. Failure-type classification is automated and approximate.

Metadata source: arXiv